Atomic Layer Deposition for the Design of Novel Catalytic Materials
MRSEC center:
Massachusetts Institute of Technology
http://mit.edu/cmse/research/seed4.shtml
IRG Number :
Seed IV
IRG Status:
Active This research studies the synthesis of novel catalysts that will enable the conversion of unconventional feedstock into useful compounds and will favorably impact other energy-related areas, such as hydrogen storage and carbon dioxide capture.